A more dramatic loss of the micropore surface area as compared to the external surface area were observed for CAT-B, CAT-C, and CAT-D. Hence, this observation indicates that the active component of CAT-A exist mainly on the external surface of the carbon support, whereas a much lower amount of the active component is present on the external surface of the carbon support for the other three catalysts.